Nickel Ceramic Bonding Alloys For Casting

NIMON EXTRA

Non-precious beryllium-free Nickel bonding alloy

Biocompatibility
Beryllium-free ceramic bonding alloy
Pure charge ingredients
Biocompatibility independently tested and confirmed by Geneva Labs, USA
Composition independently tested and confirmed by Intertek at Rolls Royce, UK
Excellent corrosion resistance

Ease of use
Excellent casting properties
Lower Vickers Hardness ensures easier polishing
Optimal ceramic bonding
Excellent surface finish
Very high corrosion resistance

nimonextra298 Nickel Ceramic Bonding Alloys For Casting

                                Composition in % by mass
                      Ni 63,5  Cr 23,0  Mo 10,5   Si < 1  Fe < 1  Ce < 1  Nb < 1

Interactive Whiteboards by PolyVision

Property Value
Density (g/cm3) 8,2
CTE 25-500 C 13,8
CTE 20-600 C 14,0
Pre-heating temperature (C) 900-1000
Casting temperature (C) 1350-1400
Melting range (C) 1220-1270
Modulus of elasticity (GPa) 200
Elongation limit (RP 0.2)(MPa) 15
Tensile strength (MPa) 800
Vickers Hardness [HV1O] after casting 220